85-95% B zili ndi Amorphous Boron Powder

85-95% B zili ndi Amorphous Boron Powder

Kufotokozera Kwachidule:

Amorphous boron ufa, womwe umadziwikanso kuti monomer boron, elemental boron, boron powder, ndi wopanda pake komanso wopanda fungo, ndipo ndi wofiirira mpaka bulauni-wakuda amorphous ufa.The mankhwala zimatha amorphous boron ufa ndi yogwira.


  • Nambala Yachitsanzo:HR-B
  • Chiyero:85%, 95%, etc
  • Mawonekedwe:ufa
  • Kukula:1-2um, 1-3um, 10um, etc.
  • Kachulukidwe:2.35g/cm3
  • Malo osungunuka:2300 ℃
  • Malo otentha:2550 ℃
  • Ntchito:Ma airbags oyendetsa magalimoto, oyendetsa rocket, ndi zina
  • Kulongedza:vacuum aluminium zojambulazo thumba
  • Tsatanetsatane wa Zamalonda

    Mafotokozedwe Akatundu

    Amorphous boron ufa, womwe umadziwikanso kuti monomer boron, elemental boron, boron powder, ndi wopanda pake komanso wopanda fungo, ndipo ndi wofiirira mpaka bulauni-wakuda amorphous ufa.The mankhwala zimatha amorphous boron ufa ndi yogwira.Ndiwokhazikika mumlengalenga ndi kutentha kwa chipinda, oxidized ikatenthedwa mpaka 300 ℃, ndipo imayaka ikafika 700 ℃.Monga mankhwala abwino a boron, amagwiritsidwa ntchito kwambiri muzitsulo, kaphatikizidwe, zakuthambo ndi zina.Amorphous boron ufa nthawi zambiri amagwiritsidwa ntchito ngati deoxidizer, woyambitsa wa airbag yamagalimoto, poyatsira mafuta oyambitsa rocket, ndi zina zambiri.

    Kufotokozera

    Amorphous Boron Powder / Boron Powder / B ufa
    Chemical Composition%
    Gulu Chiyero Mg H2O2 Insoluble Madzi Osungunuka B Chinyezi Kukula kwa Tinthu (D50)
    HR-S 85 min 11 max 1.5 max 1.0 kukula 1.0 kukula 2 umm
    HR-M 90 min 7 max 1.0 kukula 1.0 kukula 0.5 max 2 umm
    HR-G 95 min 2 max 1.0 kukula 1.0 kukula 0.5 max 2 umm

    COA

    COA

    Kugwiritsa ntchito

    Ntchito za Amorphous Boron Metal Powder:
    1. Gasi mkangazire, kusungunula chitsulo chapadera, deoxidizer yopanda okosijeni yamkuwa, chowonjezera cha njerwa za magnesia-carbon popanga chitsulo ng'anjo yotentha kwambiri.
    1. Ma airbags amagalimoto,
    2. Wothandizira roketi
    3. Chemical zinthu zokutira ndi Hardener
    4. Zoumba zamafakitale, etc.
    5. chotengera cha nyutroni mu zowongolera za nyukiliya ndi kuuma kwa radiation
    7. theka-conductor dopant

    Njira yoyendetsera bwino

    kuwongolera khalidwe
    Huarui ali ndi dongosolo lokhazikika loyang'anira.Timayesa zinthu zathu poyamba tikamaliza kupanga, ndipo timayesanso tisanaperekedwe, ngakhale zitsanzo.Ndipo ngati mukufuna, tikufuna kuvomereza gulu lachitatu kuti tiyese.Zachidziwikire ngati mukufuna, titha kukupatsani zitsanzo kuti muyese.

    Zogulitsa zathu zimatsimikiziridwa ndi Sichuan Metallurgical Institute ndi Guangzhou Institute of Metal Research.Kugwirizana kwanthawi yayitali ndi iwo kumatha kupulumutsa nthawi yambiri yoyesera kwa makasitomala.


  • Zam'mbuyo:
  • Ena:

  • Lembani uthenga wanu apa ndikutumiza kwa ife